Cellular Lightweight Concrete (CLC) – Edama Germany
Accelerated hardening of foam concrete leads to economy in the use of mould. It may be achieved by the use of certain admixtures, by using high early strength Portland cement, or by heating the moulds and the mixing water. The temperature of the mixing water should be kept above 24 °C, preferably at 30 °C, for best results. 5.0 CURING